russosborne Posted July 5, 2015 Posted July 5, 2015 http://www.amazon.com/DELUXE-MATERIALS-DLXBD044-Perfect-Plastic/dp/B0076LAVFK/ref=pd_bxgy_21_text_z I came across this stuff while looking at the Trumpeter Parting Line Engraver that was recommended in another post and this stuff was listed as a suggested "frequently bought together" from Amazon. It's water based, which is good from a health standpoint, but does it really work? Seems a tad expensive, but I don't know whether the size is comparable with other putties. If it works it would be worth it just for the no fume part to me at least. Thanks, Russ
1930fordpickup Posted July 5, 2015 Posted July 5, 2015 The reviews seem to be good news. It is not cheap but if you are only using it to fill some small seems it might not be that bad if it last a long time.
fseva Posted July 5, 2015 Posted July 5, 2015 Well, the manufacturer is in the UK - so, you're basically buying an "import". Here is their website... https://www.deluxematerials.co.uk/gb/scale-plastics/87-perfect-plastic-putty-5060243901095.html
Jon Haigwood Posted July 5, 2015 Posted July 5, 2015 Super Glue mixed with Baby Powder works for me. Gives me a chance to use up my bottles of glue with messed up caps and the glue is getting thicker.
hooknladderno1 Posted July 6, 2015 Posted July 6, 2015 http://www.amazon.com/DELUXE-MATERIALS-DLXBD044-Perfect-Plastic/dp/B0076LAVFK/ref=pd_bxgy_21_text_z I came across this stuff while looking at the Trumpeter Parting Line Engraver that was recommended in another post and this stuff was listed as a suggested "frequently bought together" from Amazon. It's water based, which is good from a health standpoint, but does it really work? Seems a tad expensive, but I don't know whether the size is comparable with other putties. If it works it would be worth it just for the no fume part to me at least. Thanks, Russ Russ, I have used it several times and LOVE it! Because it is not solvent based, it does not damage surrounding detail. I haven't had any adhesion problems. As it is NOT solvent based, NO noxious odors! It sands and feathers well - another great feature. Check out the videos on Youtube. A 40ml tube costs $7-8.00 at most hobby stores. Any LH?S that uses Horizon Hobby can get it or any of the Deluxe Materials products for you. I have no financial or material connection to this product. I am just a happy customer! David
Mike_G Posted July 6, 2015 Posted July 6, 2015 Tamiya White Putty is ~$4.50 @1.12oz. I used that on my last build and liked it- got it at Hobby Lobby with a 40% off coupon I used to use Gunze Sangyo Mr. White Putty and I liked it too, but my LHS stopped carrying it
russosborne Posted July 6, 2015 Author Posted July 6, 2015 Thanks. I may give it a try at some point. The solvent free part is a major plus for me, I have several health issues. I'm trying to go solvent free as much as possible, but I don't think that is possible for everything in this hobby. Russ
Mr Stock Posted July 6, 2015 Posted July 6, 2015 I use it mostly because Im in the UK and I wanted an alternative to Squadron which I do not like. It works great for me, smooth to apply dries fast and sands beautifully, and also as already mentioned its solvent free. Ive had a tube for over a year now and its not dried in the tube either which is good news. I use a fair amount of Deluxe products and they are very good indeed.
aurfalien Posted July 6, 2015 Posted July 6, 2015 I'm curious, it seems the Tamiya White Putty dries hard as a rock. I also find myself thinning it here and there due to quick chunkification. I've been going back and forth between it and Bondo Spot Putty but both are solvant based. Although the Bondo stuff is really cool to work with.
misterNNL Posted December 10, 2017 Posted December 10, 2017 I just got two more tubes that I ordered a few days ago and the manufacturer has corrected the only thing I did not like about it....the tube it is packaged in. The first one I got was in an oddly shaped almost triangular tube that is very difficult to hold and squeeze as it empties. The new tubes are supplied in a toothpaste style tube which will be much better. I really like the fact that is not solvent based. Clean up is simple and quick with a damp cloth instead of using lacquer thinner. I scratch build 1/25 scale travel trailers from the 1930's and '40's that have a lot of compound curves and not having the skills to create those shapes from styrene I shape them with blue house builders foam,sand to almost final shape with sanding sticks then coat the final shape with perfect plastic putty. Lacquer based putty attacks and dissolves the foam so this stuff is the perfect solution for me. It dries quickly and sands to a smooth finish.
Snake45 Posted December 10, 2017 Posted December 10, 2017 2 hours ago, misterNNL said: I scratch build 1/25 scale travel trailers from the 1930's and '40's that have a lot of compound curves and not having the skills to create those shapes from styrene I shape them with blue house builders foam,sand to almost final shape with sanding sticks then coat the final shape with perfect plastic putty. Lacquer based putty attacks and dissolves the foam so this stuff is the perfect solution for me. It dries quickly and sands to a smooth finish. Very interesting. I need to scratchbuild a nose for a B-26 bomber and have been thinking of doing something along these lines. Tell us about that "house builders foam." I was thinking to use green styrofoam from a crafts store meant to stick flowers in, shape it a little undersized, and coat it with J-B Weld. This would have the added advantage of then being very easy to hollow out to put lead nose weight into. But I'd like to hear more about your method.
crazyjim Posted December 10, 2017 Posted December 10, 2017 How does this Deluxe putty stand up to Duplicolor primers and HOK paint?
misterNNL Posted December 10, 2017 Posted December 10, 2017 4 hours ago, Snake45 said: Very interesting. I need to scratchbuild a nose for a B-26 bomber and have been thinking of doing something along these lines. Tell us about that "house builders foam." I was thinking to use green styrofoam from a crafts store meant to stick flowers in, shape it a little undersized, and coat it with J-B Weld. This would have the added advantage of then being very easy to hollow out to put lead nose weight into. But I'd like to hear more about your method. Richards..PM me your email address and I'll send some photos of the markings on the foam and the nose of the 1936 Curtiss Aerocar I am building right now. I have a friend who is a building contractor that gave me some scrap pieces. You will find the stuff at any big home improvement store like Menards or Lowe's but usually is 4' x 8' sheets and therefore more than a little awkward to handle and would equal three lifetimes supplies of the stuff.
misterNNL Posted December 10, 2017 Posted December 10, 2017 (edited) 1 hour ago, misterNNL said: Richards..PM me your email address and I'll send some photos of the markings on the foam and the nose of the 1936 Curtiss Aerocar I am building right now. I have a friend who is a building contractor that gave me some scrap pieces. You will find the stuff at any big home improvement store like Menard's or Lowe's but usually is 4' x 8' sheets and therefore more than a little awkward to handle and would equal three lifetimes supplies of the stuff. At the builders supply stores you will find this foam in the section where wall and foundation insulation materials are stocked. I use super glue to bond the foam to styrene surfaces which seems to be a very good bond. Jim, I have used rattle can primer to paint the surface with no problems.I don't use an airbrush so have no info about the use of HOK paints. Edited December 10, 2017 by misterNNL added details
peteski Posted December 11, 2017 Posted December 11, 2017 14 hours ago, misterNNL said: I really like the fact that is not solvent based. Clean up is simple and quick with a damp cloth instead of using lacquer thinner. . . . It dries quickly and sands to a smooth finish. Well, it is solvent based, but the solvent is H2O (water). Because the solvent (water) evaporates from it during the drying/hardening process, I would expect shrinkage. The 2-part putties which harden by a chemical reaction between the 2-parts are not solvent based and are non-shrinking.
misterNNL Posted December 11, 2017 Posted December 11, 2017 7 hours ago, peteski said: Well, it is solvent based, but the solvent is H2O (water). Because the solvent (water) evaporates from it during the drying/hardening process, I would expect shrinkage. The 2-part putties which harden by a chemical reaction between the 2-parts are not solvent based and are non-shrinking. 7 hours ago, peteski said: Well, it is solvent based, but the solvent is H2O (water). Because the solvent (water) evaporates from it during the drying/hardening process, I would expect shrinkage. The 2-part putties which harden by a chemical reaction between the 2-parts are not solvent based and are non-shrinking. 8 hours ago, peteski said: Well, it is solvent based, but the solvent is H2O (water). Because the solvent (water) evaporates from it during the drying/hardening process, I would expect shrinkage. The 2-part putties which harden by a chemical reaction between the 2-parts are not solvent based and are non-shrinking. 8 hours ago, peteski said: Well, it is solvent based, but the solvent is H2O (water). Because the solvent (water) evaporates from it during the drying/hardening process, I would expect shrinkage. The 2-part putties which harden by a chemical reaction between the 2-parts are not solvent based and are non-shrinking. 8 hours ago, peteski said: Well, it is solvent based, but the solvent is H2O (water). Because the solvent (water) evaporates from it during the drying/hardening process, I would expect shrinkage. The 2-part putties which harden by a chemical reaction between the 2-parts are not solvent based and are non-shrinking. I guess you got me there. I would like to comment further but it's time for me pour myself a nice cool glass of "solvent" and take me morning pills.:)
misterNNL Posted December 11, 2017 Posted December 11, 2017 (edited) On 12/10/2017 at 4:18 PM, misterNNL said: Jim, I have used rattle can primer to paint the surface with no problems.I don't use an airbrush so have no info about the use of HOK paints. I just took a look at a piece of this foam I have stored in my garage due to it's size. It is marked "Scoreboard Brand" styrofoam. It is light blue in color,2" thick and I have used it for bases for 2 of my larger dioramas due to how light and strong the material is.I make cuts in it with a very sharp fish filleting knife.I have also used a water based interior wall board patching material made by DAP called "Dry Dex". It dries and sands beautifully to fill in any imperfections. I hope this helps. Edited December 14, 2017 by misterNNL detail error
Ace-Garageguy Posted December 12, 2017 Posted December 12, 2017 (edited) On 12/10/2017 at 11:39 AM, Snake45 said: Very interesting. I need to scratchbuild a nose for a B-26 bomber and have been thinking of doing something along these lines. Tell us about that "house builders foam." I was thinking to use green styrofoam from a crafts store meant to stick flowers in, shape it a little undersized, and coat it with J-B Weld. This would have the added advantage of then being very easy to hollow out to put lead nose weight into. But I'd like to hear more about your method. I often use urethane foam and epoxy mixed with microballoon to form small components than can be hollowed out. I'd be happy to send you some foam and some micro. Cheap floral foam will also work if you use epoxy. Edited December 12, 2017 by Ace-Garageguy
misterNNL Posted December 16, 2017 Posted December 16, 2017 I opened the new style tubes yesterday and the screw-on tapered applicator tip makes it extra easy to apply just the needed amount of putty where needed,wet your finger with a little solvent(water)and smooth to nearly the finished contour. Overall IMOH highly recommended.
russosborne Posted December 17, 2017 Author Posted December 17, 2017 Thanks for bringing this back up. As the OP I had totally forgotten about it. I need to get some and try it. Russ
misterNNL Posted December 20, 2017 Posted December 20, 2017 I opened the new style tubes yesterday and the screw-on tapered applicator tip makes it extra easy to apply just the needed amount of putty where needed,wet your finger with a little solvent(water)and smooth to nearly the finished contour. Overall IMOH highly recommended. Just a small update on cleaning up after using this product. We are on a short 3 day get away so I take along my portable work bench which amounts to a large aluminum briefcase filled with a current project and the necessary tools and supplies to work on it. This project is a scratch built 1/25 th scale twenty four foot 1936 Aerocar travel trailer. This has a lot of compound curves thus requiring Lots of filling and sanding. Perfect Putty fills in the gritty surfaces of the sanding sticks I use petty quickly so I need to clean out that sanding stick often.Guess what.......being water soluble it washes off under a faucet in seconds. Another positive thing.
misterNNL Posted December 25, 2017 Posted December 25, 2017 (edited) A Christmas eve "Deluxe" product update. The supplier I bought the putty from sent me an advertising email with other items they offer similar to the putty. Evidently Deluxe offers a water based epoxy sealer for wood and foam. It is called foam armour wood and foam protective coating.It Deluxe part number is DLM- DB50. Evidently it can be sanded and painted when dry. I thought those reading this column just might be interested in knowing about this......and so Merry Christmas to all !! Edited December 25, 2017 by misterNNL
Mike999 Posted December 28, 2017 Posted December 28, 2017 Here's a tip on Perfect Plastic Putty that I just read in A Fine Scale-Modeling Magazine. If the PPP seems to be thickening or drying up in the tube, use an eye-dropper and put 3 or 4 drops of tap water straight into the tube. Then close the cap, shake it up and let it sit for a while. Since PPP is water-based, the water will un-thicken it. Haven't tried this yet myself, but I plan to. I have a 2-year-old tube of PPP that appears to be getting a little thick, though it's still useable. I just used it a couple of days ago to fill some small gaps and it worked fine. I sure like PPP a lot better than Squadron or Testors solvent-based putties. No smell and being water-based, it doesn't attack plastic. It stays where you put it and can be easily smoothed with a damp Q-Tip (or even a damp finger). When filling bigger gaps, I use Tamiya White or Gray putty. The Tamiya seems to dry a lot quicker than the others and, again, just behaves itself better.
Recommended Posts
Create an account or sign in to comment
You need to be a member in order to leave a comment
Create an account
Sign up for a new account in our community. It's easy!
Register a new accountSign in
Already have an account? Sign in here.
Sign In Now